- 99 LX
Dupli-Color 500 degree semi-gloss blackgarretts77 said:Looks good. Which paint did you use?
your wrinkle paint came out killer. how'd you polish the letters?
Dupli-Color 500 degree semi-gloss blackgarretts77 said:Looks good. Which paint did you use?
Thanks! I used 400 grit paper and a piece of wood for a sanding block. I took as much paint as I could off with a razor blade first, being careful not to nick the corners. The blade will cut the aluminum if you are not careful. Then I just sanded it a bit. The 400 leaves a bit of that brushed look since the grit isn't really that fine. I like it as it is, but 800 or higher would probably make it shine.Witchdoktor said:Dupli-Color 500 degree semi-gloss black
your wrinkle paint came out killer. how'd you polish the letters?
Laser03pro said:You have to heat it and pull it off.
Laser03pro said:If your going to paint something you dont want to wax it.
he didn't wax itLaser03pro said:If your going to paint something you dont want to wax it.
ahb11m said:he didn't wax it
he polished it
sorry to split hairs, but well i did...
and both products should be paint compatiable, but i wouldn't do the wax on a hot surface, without cooking it prior!!